PTFE INSIGHTS | Part 1 of 3
Explore the Series: Part 1 | Part 2 | Part 3
By Rodrigo Costa
Director of Engineering, Evantic
PTFE Defined
Polytetrafluoroethylene (PTFE) is a remarkable material. It’s resistant to almost every chemical and solvent, and it has an extremely low coefficient of friction (PTFE has the third lowest coefficient of friction of all known materials). Moisture does not affect it, nor does it degrade after prolonged exposure to sunlight. It’s non-toxic, non-flammable, and has a broad operating temperature range, from cryogenic -200°C (-238°F) up to 260°C (500°F), making it suitable for a wide range of applications. These properties are relatively independent of fabrication conditions.
The Construction of PTFE
PTFE is a synthetic fluoropolymer produced by the polymerization of the tetrafluoroethylene (TFE) monomer generating a perfluorinated1 high-molecular-weight polymer. Teflon® is a widely known brand name of PTFE, discovered by DuPont (now Chemours) in 1938. The discovery was made by accident by Dr. Roy Plunkett while researching new refrigerant gases and marked the beginning of the fluoropolymers era.
Many of the unique properties of PTFE can be explained by its molecular structure. The carbon-carbon bonds, which form the backbone of the polymer chain, and the carbon-fluorine bonds are extremely strong. The fluorine atoms form a regular, protective sheath over the chain of carbon atoms. This sheath protects the polymer molecule from chemical attack. It also reduces the surface energy, resulting in the low coefficient of friction and non-stick properties.
1 A perfluorinated compound (PFC) is an organofluorine compound containing only carbon-fluorines and C-C bonds but also other heteroatoms. PFCs have properties that result from the presence of fluorocarbons (containing only C–F and C–C bonds) and the functional group., https://www.wikipedia.org/
A Polymer for Diverse Applications
PTFE has far more applications than just coatings for cookware. Due to its chemical inertness, it is also frequently used as a liner in tanks or pipes conveying corrosive chemicals. Because of its low coefficient of friction, it is used as bearing surfaces on sliding or rotating devices. Its excellent dielectric properties enable PTFE to be used as an insulator in machinery, wire, and cable.
We will examine PTFE applications in future articles addressing various PTFE types and processing techniques.
Production of PTFE Resins
In order to produce PTFE resins, TFE is polymerized in water in the presence of an initiator, a surfactant, and other additives. Two different regimes of polymerization are common for production of the different types of PTFE. Granular resins are produced by the process known as Suspension Polymerization. These types of resins are used in the compression molding process to make rods, cylinders, sheets and other shapes. In this process, TFE is polymerized in a very small amount of water with high agitation. Fine Powder and Dispersions are produced by the process known as Emulsion or Dispersion Polymerization. Fine powder resins are used in the paste extrusion process to make rods, tubes and films. This type of resin is also called coagulated dispersion, which relates to the finishing steps in the manufacturing process. Dispersion polymerization is carried out with a higher amount of water and mild agitation in contrast to the suspension process. While dispersion and fine powder products are polymerized using the same method, different finishing steps are required.
According to Ebnesajjad, “the TFE monomer polymerizes linearly without branching which gives rise to a virtually perfect chain structure up to rather high molecular weights” [1]. Because of the way TFE is polymerized, the PTFE polymer has a very high molecular weight (106 – 107 g/mol for commercial applications). This very high molecular weight is necessary so PTFE products with useful properties can be made.
PTFE, a Heavyweight Fluoropolymer
One consequence of the very high molecular weight of PTFE is its very high melt viscosity. In its molten state, PTFE viscosity is around 1011 – 1012 poise (at 380°C) and therefore, develops no flow upon melting. As a comparison, motor oil SAE60 has a viscosity of 10 – 20 poise (at room temperature) and FEP’s (another fluoropolymer) viscosity is approximately 105 poise (at much lower temperature, 260°C). The closure of voids in articles made from PTFE does not happen as easily and completely as in other plastics. Voids affect permeation and mechanical properties such as flex life and stress crack resistance.
To improve the mechanical properties and resistance to permeation, these residual voids must be eliminated. This can be done by reducing the viscosity without introducing too much recrystallization. The solution has been to introduce a small amount of a comonomer with tetrafluoroethylene during the polymerization process to disrupt the structure of PTFE. Commercial PTFE resins include homopolymers and copolymers. The normal convention of polymer science applies the name copolymer to any fluoropolymer resin containing more than 1% of a comonomer. If no comonomer is used in the polymerization process, the fluoropolymer is called virgin homopolymer. A fluoropolymer containing less than 1% comonomer is categorized as a modified homopolymer resin. Examples of comonomers include perfluoromethyl vinyl ether (PMVE), perfluoroethyl vinyl ether (PEVE), perfluoropropyl vinyl ether (PPVE), hexafluoropropylene (HFP), CTFE and perfluorobutyl ethylene (PFBE).
If you are looking for more information on PTFE-based parts, visit www.evantic.com or contact us at sales@evantic.com.
REFERENCES
[1] Ebnesajjad, Sina. Fluoroplastics: Non-Melt Processible Fluoroplastics, the Definitive User’s Guide and Databook. Vol. 1, Plastics Design Library, 2000.
[2] DuPont. Teflon PTFE: Properties Handbook. Teflon PTFE: Properties Handbook, DuPont, 1996.